Checking
Hairline surface cracks in an HMA mat caused by steel wheel rollers. Usually a result of over-compaction or attempting to compact the mat below cessation temperature.
Hairline surface cracks in an HMA mat caused by steel wheel rollers. Usually a result of over-compaction or attempting to compact the mat below cessation temperature.
Absolute Viscosity (also Called 'dynamic Viscosity')
Air Traffic Control Tower (ATCT)
Alligator Cracking (also Called 'fatigue Cracking')
Consensus Requirements (properties)
Dynamic Viscosity (also Called 'absolute Viscosity')
Fatigue Cracking (also Called 'alligator Cracking')
Flushing (also Called 'bleeding')
Rice Density (also Called 'TMD')
Security Identification Display Area (SIDA)
Specification, Proprietary Product
Specification, Statistical Acceptance
Thermal Cracking (also Called 'transverse Cracking')
TMD (also Called 'Rice Density')
Transverse Cracking (also Called 'thermal Cracking')